#1 ·
If yes, what product?

I haven’t had much success.
 
Discussion starter · #6 · (Edited)
Yes it works for flux core…I’ve used 3 different brands, and they all did fine. A good coating will allow you to take a putty knife or some thin metal and knock any slag & bb’s right off the weld area.

Oh, I guess i have lived an entitled life. I was kinda expecting it to not be there. I guess it does work for me.

I currently have a weldaid spray. Works well for mig.
 
Discussion starter · #11 ·
I thought anti spatter/cooking spray was for fcaw. So what do you use it for, TIG and SprayTransfer or globular transfer or 7018. Don't tell me it's for 6010 because that would mean I'm welding wrong ? Joking but seriously, isn't anti spatter for fcaw only ?
I thought it was for fluxcore too. I use to for mig. Spray tables, fixtures and weldment.