So here is the deal guys.. Recently, due to financial issues, im going to have to start work as welder. My dad is a top notch welder and a welding instructor. I welded sparingly about 7 or 8 years ago and recently began going to work with ole dad. Ive been in about two weeks and i have picked it up at an alarming rate. I started out running 7018 on a flat plate with pretty good results and quickly moved to vertical, overhead, etc. My dad only had to demonstrate each process one time . I learned the weave in one day after only being shown once. Ok so now i feel on top of the world, Im a natural right? Well this was until yesterday. Ole dad is outta town till monday and yesterday in the shop i stumbled onto old number 6010. Hmm, I thought to myself, ill look up the ranges for it and see what its like. I was familiar with the rod only because i remembered it being used in info i read about pipe work etc. Well I absolutely hate this Fn rod. I been practicing since yesterday and i can do the whip but i have really hated the rod all around. Spattering , Stinking, Flaming POS IMO. I know the all roots in pipe are basically 6010 and im thinking i do not wanna hafta run this crap all the time. Any advice guys? Seems like someone would have come up with a something better by now to replace it. Hopefully dad can help me out monday but this rod makes me very uneasy and as always i like all the input i can get.