Disclaimer: Everything i know on this subject was learned in the past 2 weeks. I’m open to all criticism.
Decided I want to learn more about hydraulics, so I am going to replace my 20t
Swag off-road finger brake (19” long) with a 36” long capacity.
Rounding up it will have 40Tons of downforce. Powered by a car lift power unit at 2950psi.
Main parts are 1” X 6” cold rolled. The middle of the press blade is 10” to the top of the hat shape. It “should” be grossly overbuilt”
I drew this design from from the ground up with my limited knowledge on the subject.
The biggest hurdle is timing the cylinders, I’m not going for extreme precision but I do want it pretty good. I plan to use a geared flow divider to hopefully Achieve “good enough.”
Stroke will be 6”, no need for it to be that long but it gives me the option to move the blade out of my way.
Anyway, stay tuned. Steel is ordered.
I estimate the project to cost about $3000 and whatever after for tooling etc.
View attachment A085709F-8063-4C83-82D8-7954D2E99CE0.jpeg
View attachment F54F7EF7-0B42-4416-9946-B9CABB4375F4.jpeg
View attachment AE0BFDC8-5BA2-4B51-B1D1-61BDA5765ED8.jpg
Decided I want to learn more about hydraulics, so I am going to replace my 20t
Swag off-road finger brake (19” long) with a 36” long capacity.
Rounding up it will have 40Tons of downforce. Powered by a car lift power unit at 2950psi.
Main parts are 1” X 6” cold rolled. The middle of the press blade is 10” to the top of the hat shape. It “should” be grossly overbuilt”
I drew this design from from the ground up with my limited knowledge on the subject.
The biggest hurdle is timing the cylinders, I’m not going for extreme precision but I do want it pretty good. I plan to use a geared flow divider to hopefully Achieve “good enough.”
Stroke will be 6”, no need for it to be that long but it gives me the option to move the blade out of my way.
Anyway, stay tuned. Steel is ordered.
I estimate the project to cost about $3000 and whatever after for tooling etc.
View attachment A085709F-8063-4C83-82D8-7954D2E99CE0.jpeg
View attachment F54F7EF7-0B42-4416-9946-B9CABB4375F4.jpeg
View attachment AE0BFDC8-5BA2-4B51-B1D1-61BDA5765ED8.jpg