Hi all,

I'm wondering if there's a difference between the Diagnol vs Square hole layout on welding tables? Is one more advantageous than the other or do they each have their benefit/purpose?

I'm wondering which I should choose. Some explanation would help me decide.

Thanks all,

Av
 
#5 ·
I have this 2'x4' table from weldingtables.com



with 16mm holes on a 2" grid pattern



which can also be used on the diagonal with holes spaced 2.8284" apart (2 x sqrt(2))



works the same way to get a square grid on a diagonally laid out table

with either, you can line things up parallel or 45 degrees to an edge.
 
#8 ·
Perhaps a better question might be, does anybody using one of these tables hits dead spots with tooling?

My shop built table has dimension where the my clamps will not reach. I am guessing there is a relationship between the holes and clamp reach. In just modded some cheap bessey clamps to work for my table.