Is it possible to weld aluminum with an AC-225 stick. I have done some research and I have found that some say you can and some say you cant. If its possible what electrode should be used? Any help would be appreciated.
P pulser · Registered Joined Nov 2, 2005 · 1,707 Posts #2 · Jan 17, 2007 View full thread I have heard it's possible, but not easy to make quality aluminum welds with SMAW (stick welding). A quick search brought up Harris alloy #26. http://www.harrisproductsgroup.com/consumables/catalogsection.asp?Category=alum_elect Give it a go, and let us know how it works.
I have heard it's possible, but not easy to make quality aluminum welds with SMAW (stick welding). A quick search brought up Harris alloy #26. http://www.harrisproductsgroup.com/consumables/catalogsection.asp?Category=alum_elect Give it a go, and let us know how it works.