SUB ARC WELDING

339 views 4 replies 4 participants last post by  133341  
#1 ·
please we use corimpex sub arc machine for welding on beam nowdays we receive a lot of pieces with undercut full lenght through welding parametre setting is correct someone can help please
 
#5 ·
Well, it would be nice if we knew what type of weld joint we’re talking about. I’ll assume fillet weld. If you’re getting undercut, you need either more wire or less voltage, or maybe slow down the travel speed.