Sandblasting may be a no-no for aluminum. Has anybody tested other media? I've seen crushed walnut shells used for very gentle media blasting. Inquiring minds want to know...
I would NOT advise media blasting any Aluminum with anything..
Not so much the media but the crap that has been removed mixes with the media will cause problems..
That's if you use a blasting cabinet that reclaims the media..

Just stick with the Grinder/Stainless Brush and Acetone...
Why go looking for problems?....:nono:

...zap!
 
Interesting..

I'm no scientist but that is a "Non Issue" amount per length of filler...


Back to the orig question.
Sandblasting Aluminum before welding is a :nono:


...zap!
 
Yes, that "sand" is already alloyed with your filler, .


And how exactly does this happen to Aluminum alloy wire?
Unless you drop in on the beach beforehand..?

I don't have ANY of what is going on in this thread going on in my welds at any time...:confused:

And I can push 3/32" Red over 250 amps...



Nice Demo Papabear..:drinkup:

...zap!
 
SAND blasting will impregnate into ALUMINUM so that is NOT an option...

Steel ..Well just make it REAL clean after before continuing..