Hey, pretty much always used 75/25 or straight co2 gas. I've heard 85/15 or 90/10 runs smoother, is that correct? It would be nice to have it if It runs nice short circuit and the odd times I want to spray arc it will work great for that. Does it suffer on short circuit compared to the C25?
They have 92/8 as well but couldn't see it being any better.
They have 92/8 as well but couldn't see it being any better.